默认 yield stress for old reinforcing bars

yield stress for old reinforcing bars
i'm evaluating some concrete beams that were designed in 1926. any idea what the yield stress for reinforcing bars from that era is?
find a job or post a job opening
without any additional info. or rebar tests, i would not recommend using a yield greater than 33 ksi.
i suggest that you order a copy of "evaluation of reinforcing bars in old reinforced concrete structures", engineering data report number 48 by crsi.
grades:
structural 33,000 psi
intermediate 40,000 psi
hard 50,000 psi
my 1937 copy of trautwines civil engineers reference book gives:
"normal reinforcing steel ultimate strength of between 50,000 - 70,000 lbs per sq in with elastic limit (yield) at 25,000 - 35,000 lbs per sq in.
cold working the bars will raise the elastic limit to 40,000 - 50,000 lbs per sq in.
deformed bars have a higher elastic limit claimed at 50,000 - 65,000 lbs per sq in."
i pulled this information off the internet some time ago. it actually came from a post on eng-tips.
hope it helps.
per fema 356 table 6-1, rebar typically came in 3 grades prior to 1968:
structural: fy = 33 ksi, fu = 55 ksi
intermediate: fy = 40 ksi, fu = 70 ksi
hard: fy = 50 ksi, fu = 80 ksi
the following info is per crsi engineering data report no. 48:
hard grade is referred to reinforcing with fy = 50,000 psi. and fu = 80,000 psi.
intermediate grade is referred to reinforcing with fy = 40,000 psi and fu = 70,000 psi.
structural grade is referred to reinforcing with fy = 33,000 psi and fu = 55,000 psi.
these are tied into the following astm's:
1911-1966 - astm a15 (billet steel) (all three grades)
1913-1966 - astm a16 (rail steel) (hard grade only)
1936-1964 - astm a160 (axle steel) (all three grades)
i think you can get this document from www.crsi.org
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
yield stress and steel design huangyhg 产品功能分析 0 2009-09-16 11:45 PM
stress for tubing huangyhg 产品功能分析 0 2009-09-16 10:38 AM
residual stress in bent steel huangyhg 产品功能分析 0 2009-09-15 06:22 PM
impact loads and strain rate dependent yield stress huangyhg 产品功能分析 0 2009-09-09 07:13 PM
calculating reinforcing actual stress huangyhg 产品功能分析 0 2009-09-07 10:03 PM


所有的时间均为北京时间。 现在的时间是 03:05 PM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多