默认 fillet weld strength

fillet weld strength
i have always known that the allowable shear stress of a fillet weld to be based on its effective throat thickness and the allowable stress equal to (.707)(.30)(70). is this the same when the weld is loaded perp. to the longitudinal axis of the weld and is it is in tension?
check out our whitepaper library.
when you have such a case, shouldn't you use butt weld or other full penetration welds rather than designate fillet weld, which i don't see how could it be.
the weld is 50% stronger when loaded perpendicular to its longitudinal axis. you still have shear on the effective throat.
nutte,
where can i find this written? is it in the asd manual?
you might try looking in blodgett...
mike mccann
mmc engineering
it's not in the green asd manual. it is a "new" development since that manual was released.
look at equation j2-5 on page 16.1-100 in the 13th black manual. it's the term with the sin theta in it that gives you 1.5 when perpendicular.
it's in the 3rd lrfd manual on page 16.1-115.
it first appeared in the 2nd lrfd manual.
thanks nutte!!!! i am so used to the 9th edition that i am still getting used to the 13th. so let me get this straight based on a 1/4" fillet:
theta = 90 degrees
aw = .707(1/4)=.1768in
so: fw = .60(70ksi)(1.5)=63ksi

rn = (63ksi)(.1768in) = 11.14k/in
11.14 k/in / 2 = 5.56 k/in allowable
parrallel to axis = (.707)(70)(.30)(1/4) = 3.71 k/in
5.56 k/in / 3.71 k/in = 1.5
thanks nutte, makes sense now. that was a big help

for e70 electrodes, i always have figured 900# per 1/6" of weld, per inch of weld, or about 3600# per inch with a 1/4" weld. (parallel to axis)
for e60, use 2/3 of that.
mike mccann
mmc engineering
i think it's newish to the aisc code, but has been known through testing for near on 100 years. the aisc design guide 21 discusses this.
regards,
ys
b.eng (carleton)
working in new zealand, thinking of my snow covered home...
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
 


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
determining required weld strength huangyhg 产品功能分析 0 2009-09-08 06:28 PM
concrete compressive strength huangyhg 产品功能分析 0 2009-09-08 11:53 AM
analysis of an over-weld huangyhg 产品功能分析 0 2009-09-07 11:35 AM
10 ft continuous weld beam to cover plate huangyhg 产品功能分析 0 2009-09-06 10:26 PM
【转帖】ack weld a nu yang686526 American standards 0 2009-05-04 10:37 AM


所有的时间均为北京时间。 现在的时间是 06:09 PM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多