welding titanium
i will be autogenously welding .125 in. thick cp grade 2 titanium using the gtaw process. the surrounding atmosphere will be purged with argon. i know that the weld must be cooled to below 800 degrees f before entering the atmosphere. my question is: "is it possible to cool the weld too quickly?".
the weldment will be post weld heat treated after welding.
will the weld crack etc... if it is cooled to fast?
thanks in advance!
check out our whitepaper library.
in our welding of titanium as you state we let the weld cool under purge gas to 800f max, normally 600f. we then pull the purge and let the material air cool and have never had a problem. i have seen some pretty bad ti welds in grade 2 material and have never seen any cracking when cooling from welding temperature. another thing is that a ti weld is cooled fairly rapidly by the trailing shield, normally well below the 800f mark. we are looking for corrosion resistance and not necessarily high strength so we never heat treat ti.
is your heat treatment a stress relief or an anneal?
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
heat treat titanium 96al-4v0 huangyhg 精密机械 0 2009-09-05 10:54 PM
plastic welding strength test standards huangyhg ISO standards 0 2009-09-05 07:21 PM
ansi 9standards0 code issues - welding end preparation a huangyhg American standards 0 2009-09-05 06:02 PM
welding specification in drawings huangyhg tec-ease(America) 0 2009-09-05 01:53 PM
【转帖】welding specification in drawings yang686526 American standards 0 2009-05-04 11:13 AM


所有的时间均为北京时间。 现在的时间是 04:18 PM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多